Minimum Physical Properties for Copper Alloys Group B & C
|
GROUP B
REFRACTORY METALS
|
HARDNESS
ROCKWELL
(HRB) **
|
CONDUCTIVITY
% I.A.C.S. ***
|
ULTIMATE COMPRESSIVE STRENGTH
ksi
|
|
CLASS 10
|
ROD, BAR, INSERTS
|
72 HRB
|
45%
|
135
|
|
CLASS 11
|
ROD, BAR, INSERTS
|
94 HRB
|
40%
|
160
|
|
CLASS 12
|
ROD, BAR, INSERTS
|
98 HRB
|
35%
|
170
|
|
CLASS 13
|
ROD, BAR, PLATE, INSERTS
|
69 HRB
|
30%
|
200
|
|
CLASS 14
|
ROD, BAR, PLATE, INSERTS, TUBE
|
85 HRB
|
30%
|
88
|
|
GROUP C
DISPERSION STRENGTHENED COPPER
|
HARDNESS
ROCKWELL
(HRB) **
|
CONDUCTIVITY
% I.A.C.S. ***
|
YIELD STRENGTH ksi
Typical
(0.2% Offset)
|
ULTIMATE
TENSILE
STRENGTH
ksi
|
ELONGATION %
IN 1” GAUGE
(Typical)
|
|
CLASS 20
|
ROD, BAR, PLATE
|
75 HRB
|
75%
|
75
|
80
|
20
|
RWMA Table 1.8.4
* Conductivity = 1/.0058 (Resistivity) where: Conductivity is expressed in the units % IACS and resistivity is expressed in the units mWcm
|